knunchakaman
- 6
- 1
Honestly I left this part up to my buddy. It involves measuring temperatures and doing timed stuff. Lots of dry ice. It's a whole science project. I'd have to pay my buddy to set it up and show me. But yeah. It all needs to be made up to snuff. You don't want a leak. Or worse.do i need to freeze the tube and material also before I introduce the cold solvent? Its a lot of trouble to chill the tubes and material…easy to chill the solvent down… If I get my solvent chilled to -70 … I know my material isnt holding many btu…maybe some btu in the metal tube but not much…….do i need to get tube with the material to -70 also? Im sure it will get there as soon as the solvent hits it.
You probably need to check with the manufacturer. Like I said I have to hire a guy. And the dry ice was for the outside of the machine. I don't know how it all works.I have closed jacketed material tubes. So I cant put dry ice into the tubes. This machine runs 8lbs per tube. I have 3 tubes
This is more of a growers forum. I believe you would be better off on an extractors forum.Does anyone know if this BHO machine will work better if I set up for reverse flow through the material also or can I just shoot in one direction and get as good results? I know you dont want channeling. Do I need to pack my material densely? And Does flow direction matter when your extracting material?
I have a machine that I need to set up so that I will produce some quality extract. It has 3 x 6”ID closed jacketed tubes ….a large jacketed gas receiving tank with a cooling coil….and a 12”jacketed receiving vessel. Ill send some pics….but I need to figure out how to get it all cold…and add crc filtering to
We use cookies and similar technologies for the following purposes:
Do you accept cookies and these technologies?
We use cookies and similar technologies for the following purposes:
Do you accept cookies and these technologies?